Effect of different post-curing times on the physicomechanical properties of 3D-printed resins intended for permanent restorations

Sep 2026 · Journal of Clinical and Experimental Dentistry · Vol 18, pp. e1164 - e1172 · 0 citations · 13 references
Medicine

TL;DR

Post-curing time influenced the physicomechanical properties of 3D-printed resins intended for permanent restorations, with the response depending on the material and property evaluated.

Abstract

Background Three-dimensional (3D)-printed resins intended for permanent restorations represent a promising alternative to conventional restorative materials. Although the effect of post-curing duration on these materials has already been investigated, material-specific evidence for some recently developed resins remains limited. This study aimed to evaluate the effect of different post-curing times on the surface microhardness, flexural strength, and fracture resistance of these resins. Materials and Methods An in vitro experimental study was conducted using three 3D-printed resins (VarseoSmile TriniQ, Prizma 3D Bio Crown Diamond, and Prizma 3D Bio Crown) and a CAD/CAM nanohybrid resin (Evolux Hybrid) as the reference group. The printed resins were subjected to three post-curing times: Half the manufacturer-recommended time, the recommended time, and twice the recommended time. Surface microhardness, flexural strength, and fracture resistance were evaluated. Data were analyzed using two-way analysis of variance and the Bonferroni post hoc test (α=0.05). Results Material type, post-curing time, and their interaction significantly affected the physicomechanical properties evaluated (p<0.05). For VMH, the highest values were recorded for Bio Crown Diamond-T3 and VarseoSmile TriniQ-T3, at 23.59 ± 1.58 and 23.47 ± 1.17, respectively, with no significant difference between them. VarseoSmile TriniQ-T3 exhibited the highest flexural strength and fracture resistance values, reaching 128.14 ± 11.35 MPa and 933.14 ± 20.77 N, respectively. Bio Crown showed the lowest values for all three properties evaluated. Conclusions Post-curing time influenced the physicomechanical properties of 3D-printed resins intended for permanent restorations, with the response depending on the material and property evaluated. VarseoSmile TriniQ exhibited the highest flexural strength and fracture resistance. In contrast, Bio Crown Diamond achieved surface microhardness comparable to that of VarseoSmile TriniQ only after post-curing for twice the recommended duration.

Read PDF

Similar papers

Open access Oct 2026

Effect of Post-Curing Time on the Color Stability of 3D-Printed Hybrid Resin Material, an In Vitro Study

Objectives: This study investigated the effect of post-curing time on the color stability of a non-polished, as-printed hybrid 3D printed resin material and assessed whether a nitrogen atmosphere during post-curing has any influence. Methods: The 3D-printed specimens were divided into four groups based on the post-curi...

Nisrine Khneisser, L. Hardan, Z. Salameh et al. · 0 citations
Open access Oct 2026

Surface Roughness and Color Stability of 3D-Printed Dental Resin Materials Under the Influence of Different Beverages

Aim: This study aimed to evaluate the effects of the material type and immersion solution on the color stability (ΔE) and surface roughness change (ΔRa) of provisional dental materials fabricated using subtractive milling or additive 3D printing techniques. Materials and Methods: Three provisional restorative materials...

W. Ahmed, Amr Ahmed Azhari, B. N. Alturki et al. · 0 citations
Open access Jan 2026

Influence of Polishing Treatment on the Topography of 3D‐Printed Provisional Resins: An In Vitro Study

Although 3D‐printing has been increasingly integrated in the fabrication of provisional restorations, the evidence regarding the impact of different polishing regimens on their topographical features is unclear. This in vitro study assessed the outcomes of different polishing treatments on roughness measurements of 3D‐...

Yousif A. Al-Dulaijan, Abdulrahman Mohammad Aldossari, Abdulrahman Salem Bin-Jabair et al. · 0 citations
Open access Sep 2026

Effect of Storage Time on the Dimensional Stability of 3D Printed Dental Model Resins

The aim of this study was to evaluate the effect of storage-induced aging on the dimensional stability of two 3D printed resins, a plant-based and a conventional dental model resin. Sixteen dental models were fabricated from a maxillary typodont CAD reference file using two resin types (n = 8 each): a conventional resi...

M. Sadoon, A. al-Omari, O. A. Sheet · 0 citations
Open access Sep 2026

Comparative effect of polishing and coatings on the surface properties of 3D-printed denture-base resin and teeth: an in vitro study

Surface roughness of 3D printed DBR and denture teeth decreased after polishing and coatings, and coating using OG resin improved the hardness of DBR and denture teeth.

Yousif A. Al-Dulaijan, Alawiyyah Alsayed, Mashael T. Alhejji et al. · 0 citations