Skip to content
Open access

Effect of filler particle size on the printability, physicomechanical and adhesion properties of highly filled experimental 3D-printed dental resins.

Oct 2026 · E -journal of dentistry · pp. 107130 · 0 citations · 27 references
Medicine

TL;DR

Reducing filler particle size in highly filled 3D-printed resins may improve initial mechanical behavior and reduce surface roughness but these mechanical advantages were not maintained after thermocycling and were accompanied by substantially longer fabrication time.

Abstract

Purpose

The purpose of this study was to evaluate the effect of filler particle size on the printability, mechanical behavior, and surface properties of highly filled experimental 3D-printed dental resins before and after thermocycling. MATERIAL AND

Methods

Two highly filled experimental resins containing silanized barium glass with different particle sizes were formulated: microparticulated (1.5 µm) and submicroparticulated (0.7 µm). Specimens were additively manufactured by digital light processing and subjected to flexural strength (FS), elastic modulus (EM), Vickers microhardness (VHN), surface roughness (Ra), contact angle (θ), and shear bond strength (SBS) analyses before and after thermocycling (5000 cycles; 5°C-55°C). Printing time was also evaluated. Data were analyzed by independent t-test, 2-way ANOVA and Tukey tests (α=.05).

Results

The 0.7-µm formulation required significantly longer actual fabrication time than the 1.5-µm formulation (122.37 ± 12.10 versus 48.23 ± 2.96 min; p<.001). Before thermocycling, the 0.7-µm formulation showed significantly higher FS (p=.012) and EM (p<.001) but these differences were not maintained after aging. Thermocycling significantly reduced FS in both formulations (p<.001). The 0.7-µm formulation exhibited lower Ra and higher contact angle values than the 1.5-µm formulation, whereas no significant differences were observed for VHN or SBS. No significant formulation × aging interactions were detected for any evaluated property.

Conclusions

The 0.7-µm formulation showed higher initial flexural strength and elastic modulus and lower surface roughness. However, the mechanical differences were not maintained after thermocycling and no advantages were observed for microhardness or shear bond strength. These changes were accompanied by substantially longer fabrication time. CLINICAL

Significance

Reducing filler particle size in highly filled 3D-printed resins may improve initial mechanical behavior and reduce surface roughness but these mechanical advantages were not maintained after thermocycling and were accompanied by substantially longer fabrication time.

Read PDF

Similar papers

Open access Sep 2026

Effect of air-borne particle abrasion and tribochemical silica coating on surface characteristics, mechanical behavior, and bonding performance of 3D-printed resin-based materials

This study evaluated how air-abrasion material, application time, and aging affect the surface characteristics, mechanical behavior, and bonding performance of three-dimensionally (3D) printed resin. Specimens were treated with aluminum oxide (Al₂O₃) or tribochemical silica coating (SiO₂) for 5, 10, and 15 s (50 μm, 2...

R. Dascanio, B. S. H. Tonin, Isabella Gama et al. · 1 citation
Open access Sep 2026

Effect of printing temperature on the viscosity, photopolymerization, and mechanical properties of a highly filled 3D-printing dental resin composite.

OBJECTIVE This study aimed to evaluate the effect of three printing temperatures on the viscosity; cure depth (Cd) and working-curve parameters (Dp, Ec); degree of conversion (DC) and polymerization kinetics; and post-cured flexural strength (FS), flexural modulus (FM), and the Weibull reliability of flexural strength...

Ulysses de Toledo Monteiro, A. Correr, M. Rocha · 0 citations
Open access Sep 2026

Flexural Performance and Surface Hardness of Filler-Modified PMMA Designed for Denture Base Applications

Polymethyl methacrylate (PMMA) is widely used in denture base fabrication; however, its relatively low flexural strength (FS) and durability limit long-term clinical performance. Reinforcing with nanofillers such as Halloysite nanotubes (HNTs) has emerged as a promising strategy to enhance the material's mechanical p...

Rugaia Sharef, William Thomas, Hazizan Akil et al. · 0 citations
Open access Sep 2026

Effect of different post-curing times on the physicomechanical properties of 3D-printed resins intended for permanent restorations

Post-curing time influenced the physicomechanical properties of 3D-printed resins intended for permanent restorations, with the response depending on the material and property evaluated.

José Giancarlo Tozo-Burgos, M. Sánchez-Tito, John Alexis Dominguez · 0 citations
Open access Sep 2026

Comparative effect of polishing and coatings on the surface properties of 3D-printed denture-base resin and teeth: an in vitro study

Surface roughness of 3D printed DBR and denture teeth decreased after polishing and coatings, and coating using OG resin improved the hardness of DBR and denture teeth.

Yousif A. Al-Dulaijan, Alawiyyah Alsayed, Mashael T. Alhejji et al. · 0 citations
Open access Oct 2026

Influence of surface-conditioning strategies on the shear bond strength of veneering ceramic to aged and non-aged zirconia frameworks fabricated with milling and 3D-printing

PURPOSE The purpose of this in vitro study was to investigate how various surface-conditioning strategies and thermal aging affect the shear bond strength (SBS) of aged and non-aged zirconia frameworks fabricated through different techniques. MATERIALS AND METHODS A total of 208 rectangular frameworks were fabricated b...

Selin Çakır, O. Onoral · 0 citations

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.