Interfacial evolution and cracking mechanism of TC4/AlSi12 bimetallic structures prepared by laser melting deposition
Abstract
Due to the significant differences in physical and chemical properties between titanium alloys and aluminum alloys, the formation of brittle intermetallic compounds (IMCs) is inevitable during the metal bonding process, which seriously affects the service performance of TC4/AlSi12 bimetallic structures (BS) manufactured by laser melting deposition (LMD). In this study, single-layer single-pass AlSi12 was deposited on TC4 substrates with different laser powers and scanning speeds to reveal the effects of process parameters on the microstructure, IMC development, and cracking behavior. The results show that high heat input leads to excessive melting of TC4, generating a large number of brittle IMCs such as Ti3Al, TiAl, TiSi2, and Ti5Si3, thereby inducing severe transgranular cracks at the interface. With the decrease of heat input, the quantity and size of hard and brittle IMCs decrease significantly, and the crack sensitivity is gradually suppressed. When the laser power is reduced to 1.6kW, the cracks are completely eliminated. Further reducing the power to 1.2kW can minimize the IMC content and ensure excellent defect-free metal bonding.