Sep 2026· Journal of Colloid and Interface Science· Vol 728, pp.
141656
· 0 citations· 56 references
Medicine
Abstract
The practical deployment of aqueous zinc-ion batteries (AZIBs) is severely hindered by disordered zinc deposition and water-induced parasitic reactions, which degrade the long-term cycling stability of Zn anodes. Herein, a poly(1,3-dioxolane) (PDOL) protective layer is rationally constructed on the zinc surface via a facile one-step pre-polymerization strategy. The abundant ether oxygen sites of PDOL can strongly coordinate with Zn2+ to reorganize the solvation sheath, effectively weakening water competition and suppressing the hydrogen evolution reaction (HER). Meanwhile, the PDOL interlayer homogenizes interfacial Zn2+ flux and alleviates localized current concentration, inducing preferential growth of the Zn (002) crystal plane and restraining dendrite proliferation caused by the tip effect. Furthermore, a robust organic-inorganic hybrid SEI film enriched with Zn-O/Zn-F inorganic phases is in-situ generated during cycling, which further accelerates interfacial ion kinetics and passivates the reactive zinc surface. Benefiting from the synergistic effects of solvation modulation, water confinement, and interfacial reconstruction, the PDOL@Zn symmetric cell achieves an ultra-long lifespan of over 2000 h at 10 mA cm-2 (1 mAh cm-2). Both coin and pouch full cells deliver prominently enhanced cycling durability. This work provides a facile and reliable interfacial engineering strategy toward high-stability aqueous zinc-ion batteries.
Interfacial instability at the Zn anode represents a major obstacle to the advancement of aqueous zinc-ion batteries (AZIBs), as it triggers nonuniform Zn deposition and various parasitic reactions. This study investigates the influence of alizarin red S (ARS), an organic molecule featuring an extended π-conjugated fra...
Qu Yue, Jun-Hui He, Yu-Hang Chen et al.· Energy Materials· 0 citations
The practical application of aqueous zinc-ion batteries (AZIBs) is severely limited by water-induced issues, such as hydrogen evolution reaction, Zn metal corrosion, and cathode dissolution. To simultaneously stabilize the Zn anode and the NaV3O8 (NVO) cathode, we propose a synergistic strategy based on mixed organic p...
Aqueous zinc-ion batteries (AZIBs) offer considerable potential for sustainable energy storage; however, dendritic growth and interfacial parasitic reactions severely hinder the reversibility of zinc anodes. Herein, we report a multifunctional hybrid protective interphase (PVA/ZIF-8@Zn) constructed by combining poly(...
Zhi-Ping Xiong, Yu-Liang Liu, Feng-Yuan Fu et al.· Energy & Fuels· 0 citations
Aqueous zinc-ion batteries possess intrinsic operational safety, low cost and scalable application potential, making them promising candidates for large-scale energy storage. However, Zn metal anodes still suffer from severe dendrite proliferation, hydrogen evolution, interfacial corrosion, and inevitable by-product ac...
Jing-Wei Liu, Xin-Yi Chen, Yi-Dong Huang et al.· ACS Applied Materials and In...· 0 citations
Aqueous zinc-ion batteries (AZIBs) are promising candidates for large-scale energy storage, but their practical deployment is hindered by dendrite growth and water-induced side reactions. These challenges mainly arise from the high desolvation barrier of [Zn(H2O)6]2+, which slows interfacial kinetics and promotes irr...
Yang Song, Yang Song, Li-Wen Hu et al.· ACS Sustainable Chemistry &a...· 0 citations