Thermal-History-Mediated Defect–Microstructure–Property Evolution in Multi-Laser Powder Bed Fusion of TC11 Titanium Alloy Structures

Sep 2026 · Materials · Vol 19 · 0 citations · 35 references
Medicine

Abstract

Multi-laser powder bed fusion (PBF-ML) enables efficient fabrication of large components but introduces spatially heterogeneous thermal histories near inter-laser overlap zones. However, how global thermal-input variables and local thermal-path variations jointly affect defect evolution, microstructure, and mechanical response in geometrically constrained Ti-6.5Al-3.5Mo-1.5Zr-0.3Si (TC11) structures remains unclear. Here, TC11 arch structures were fabricated by varying laser power, scanning speed, overlap-zone position, and interlayer rotation and characterized by tensile testing, optical metallography, Scanning Electron Microscope (SEM), and fractography. Increasing laser power from 170 to 290 W increased Yield Strength (YS) and Ultimate Tensile Strength (UTS) from 955 and 1228 MPa to 1259 and 1463 MPa, respectively, while Elongation (EL) decreased from 14.7% to 3.1%. Increasing the scanning speed from 1050 to 1450 mm/s produced the opposite strength–ductility trend, whereas overlap-zone position had limited influence on strength and 67° interlayer rotation produced moderate improvements. Defect count and area fraction did not always vary synchronously, while semi-quantitative SEM analysis revealed microstructural coarsening with increasing laser power and refinement with increasing scanning speed. These results show that global thermal-input variables primarily govern the overall strength–ductility and microstructural-scale responses, whereas local thermal-path variables mainly regulate spatial defects and microstructural heterogeneity.

Read PDF

We use cookies to run the site and, with your consent, for analytics and to show ads. See our Cookie Policy.