Mode I fracture tests, with loading perpendicular to the grain and crack propagation parallel to the grain, were performed on 10 groups of laminated flattened-bamboo composite (LFBC) specimens using the compact tension (CT) method, and crack extension was monitored by VIC-3D (video image correlate, 3D) technique. Nine of the groups were interlaminar (RL) fracture considering specimen thickness (B) and initial crack length to width ratio (a/W), and one group was standard specimens for intralaminar (TL) fracture as a control. It was shown that the failure mechanism of TL fracture was fiber fracture and ground tissue damage, while RL fracture was adhesive failure accompanied by a small amount of fiber fracture. The difference in the failure mechanism determined the uncertainty of crack extension in RL, while the crack extension in TL was continuous. On this basis, different forms of load-displacement curves and load-crack curves were analyzed. In addition, a/W had no effect on the fracture toughness of RL, while the condition value of fracture toughness gradually increased and reached stability with increasing thickness B. The RL fracture toughness of LFBC obtained from the test was 20.8 MPa·mm1/2. The tensile strain field during crack extension was always concentrated at the crack tip, while the compressive strain appeared at the bottom of the specimen. An empirical equation for predicting the critical load of RL fracture was proposed by fitting to the test data.
Reliable determination of Mode I fracture toughness is essential for evaluating crack initiation and propagation in rock engineering applications such as hydraulic fracturing, underground energy storage, geothermal energy extraction, and CO2 sequestration. The Short Rod (SR) test is the only ISRM-suggested direct metho...
Rashid Hajivand Dastgerdi, Ł. Ostrowski, V. Sarfarazi et al.· Materials· 0 citations
Abstract An Original Equipment Manufacturer (OEM) produced row 1 turbine vanes by additive manufacturing (AM), using the Powder Bed Fusion-Laser Beam/Metal (PBF-LB/M) process. It is mandatory in such cases to co-print specimens for mechanical testing, such as short-time creep rupture testing. Some specimens were found...
A. Neidel, E. Thannhäuser· Praktische metallographie· 0 citations
Crack initiation and propagation in aerospace structures can compromise structural integrity and service safety, making fracture assessment an important aspect of joint design. Riveted aluminum joints are widely used in engineering structures; therefore, understanding their crack-growth behavior under different loading...
Mohammad Reza Khoshravan Azar, Amir Javadzadeh Khoei, M. Dadashzadeh· Journal of Materials Science· 0 citations
The fracture behavior of brittle rocks, like fractures in marble, is important for various engineering applications, including mining, underground facilities, hydraulic mining, and tunneling. While most of the prior work has focused on pure Mode I loading, rock structures undergo mixed-Mode I/II loading in which fractu...
Yan-Xiang Chen, En-Ping Guo, Lin-Hua Huang et al.· European Journal of Computat...· 0 citations
The effects of specimen heights on the fracture behaviors of concrete were studied by using the digital image correlation (DIC) technique. Three‐point bending tests on notched specimens with a constraint span but different depths were carried out. The horizontal strain field, horizontal displacement field, crack op...
Yan Yin, Kai Liang, Shao-Wei Hu et al.· Fatigue & Fracture of En...· 0 citations
Specimen-scale fitting can reproduce interlaminar fracture in carbon-fiber-reinforced aluminum laminates (CARALL) but obscures the physical origin of cohesive-zone parameters. We present a multiscale framework integrating molecular dynamics (MD), a representative volume element (RVE), finite element (FE) modeling, and...