Physics-guided inverse design of Co-based superalloys using machine learning and multi-objective optimization for enhanced $\gamma'$ solvus temperature
This physics-informed inverse design framework provides an efficient route for identifying high-performance Co-based superalloys and can be adapted to other advanced structural alloys.
Abstract
The discovery of next-generation Co-based superalloys with improved high-temperature stability is hindered by the vast compositional design space and complex interactions among alloying elements governing gamma-prime phase stability. This study presents a physics-informed machine learning framework for the inverse design of Co-based superalloys with higher gamma-prime solvus temperature while accounting for alloy density. Four descriptors representing atomic size mismatch (delta-MV), mixing enthalpy (Delta-Hm), electronegativity mismatch (delta-EN), and valence electron concentration mismatch (delta-VEC) were used to characterize the chemistry governing phase stability. Regression algorithms were evaluated using leave-one-out cross-validation, with Gaussian Process Regression (GPR) achieving the best performance (R2 = 0.932, RMSE = 34.7 deg C, and MAE = 25.9 deg C). The probabilistic nature of GPR enabled uncertainty-aware Bayesian optimization for exploring the uncharted composition space. Non-dominated Sorting Genetic Algorithm II (NSGA-II) and Genetic Algorithms were used to simultaneously increase gamma-prime solvus temperature and reduce alloy density. The optimization generated numerous previously unexplored Co-based alloy compositions, with predicted gamma-prime solvus temperatures of 1248-1353 deg C, including candidates approaching or exceeding the maximum value in the experimental dataset. Descriptor analysis identified atomic size mismatch and mixing enthalpy as key factors governing gamma-prime stability, while principal component analysis confirmed that the proposed alloys occupy chemically relevant descriptor regions. This physics-informed inverse design framework provides an efficient route for identifying high-performance Co-based superalloys and can be adapted to other advanced structural alloys.
An artificial intelligence framework that incorporates a physics-constrained inverse-design system (PHICS) built upon a directed acyclic graph (DAG) architecture for CPCMs, integrating interface, phase, and carrier engineering.
Dong-Liang Ding, Min-Hao Zou, Ruo-Yu Huang et al.· National Science Review· 0 citations
AI/ML is positioned not as a replacement for experiment, but as a transparent decision-support layer for narrowing high-dimensional alloy spaces and prioritising candidates for experimental validation in high-temperature energy applications.
Harikrishnan Kumarasamy· Journal of Energy Research a...· 0 citations
Composition-based machine learning for Al-Mg-Si alloys lacks generalization. A physics-informed strategy incorporating physicochemical descriptors was proposed, improving the coefficient of determination (R2) by 30% over composition-only models. Shapley additive explanations (SHAP) identified electronegativity differen...
Jun Li, Chen Su, Chen-Lu Yu et al.· Materials Research Letters· 1 citation
High-entropy alloys (HEAs) provide a broad compositional space for developing structural materials with balanced phase stability and mechanical performance. However, reliable mechanical-property prediction remains challenging because alloy chemistry, phase constitution, processing state, and model uncertainty are s...
Machine-learning interatomic potentials enable large-scale atomistic simulations of vanadium alloys relevant to fusion applications, but reliable training and validation remain challenging in multicomponent systems. Here, we develop a descriptor-based DeepMD-DPA1 potential for the V-Ti-Cr system using a two-stage workf...
G. S. Demyanov, D. Minakov, S. B. Saltykov et al.· 0 citations
We use cookies to run the site and, with your consent, for analytics and to show ads.