Effect of heat treatment conditions on the incremental hole flanging of AA6061 aluminum alloy sheets
In this study, the effect of heat treatment on the incremental hole flanging of 1.5 mm-thick AA6061 aluminum alloy sheets was experimentally investigated. Specimens were subjected to three conditions: annealed, solution treated, and artificially aged (T6). Flanging was performed using a five-stage forming strategy wi...