Researchers employed the improved Hummers' method to synthesize graphene oxide (GO) from graphite, chosen for its faster kinetics, enhanced safety, and reduced toxicity. Thermal annealing was conducted at 0°C, 200°C, 300°C, and 400°C. The acidity of GO was minimized through repeated centrifugation, rinsing, and decanti...